TiAlN composite coating
2022-11-15
composite coating TiAlN composite coating
Coating characteristics:
TiAlN (single layer)
Color: purple black
Microhardness (HV): 2800HV
Friction coefficient: 0.5
Maximum application temperature: 800 ℃
Binding force: 90N
TiAlN (composite)
Color: purple black
Microhardness (HV): 3500HV
Friction coefficient: 0.5
Maximum application temperature: 850 ℃
Binding force: > 100N
Multi alloying of coating, multi-layer composite coating, nano coating
Harder, stronger, better oxidation resistance, better film substrate bonding force, higher cutting speed, more choices for users.